| Management number | 222750557 | Release Date | 2026/05/04 | List Price | $248.40 | Model Number | 222750557 | ||
|---|---|---|---|---|---|---|---|---|---|
| Category | |||||||||
1. Use oxygen acetylene flame to heat the workpiece to 300-400 degrees Celsius. 2. then use spray gun spraying the self-fluxing alloy powder evenly sprayed on the surface of the workpiece, through the flame to melt till surface become like a glisten mirror surface, gradually moving molten position, make the alloy powder and the workpiece mutually cladding, dispersed to each other to form a binding layer firmly. Using different kinds of alloy powder, can get the abrasion resistance, corrosion resistance and other different properties of strengthened layer.